Controlled depolymerisation assessed by analytical ultracentrifugation of low molecular weight chitosan for use in archaeological conservation

通过分析超速离心法评估低分子量壳聚糖的可控解聚作用,以用于考古文物保护

阅读:1

Abstract

The heterogeneity and molecular weight of a chitosan of low molecular weight (molar mass) and low degree of acetylation (0.1) for potential use as a consolidant for decayed archaeological wood were examined by sedimentation velocity and sedimentation equilibrium in the analytical ultracentrifuge before and after depolymerisation. Sedimentation velocity before depolymerisation revealed a uniform distribution of sedimentation coefficient with little concentration dependence. SEDFIT-MSTAR analysis revealed a weight average molecular weight M(w) of (14.2 ± 1.2) kDa, and polydispersity index of ~ 1.2. Further analysis using MULTISIG revealed a distribution of material between 2 and 20 kDa and consistent with the weight average M(w). Controlled depolymerisation using hydrogen peroxide and ultra-violet radiation in an acetic acid medium reduced this to (4.9 ± 0.7) kDa, with a similar polydispersity. The depolymerised material appears to be within the range that has been predicted to fully penetrate into archaeological wood. The consequences for this finding and the use of the analytical ultracentrifuge in wood conservation strategies are considered.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。