Abstract

The combination of gelatin and hydroxyapatite (HA) has emerged as a promising strategy in dental tissue engineering due to its favorable biocompatibility, mechanical properties, and ability to support cellular activities essential for tissue regeneration, rendering them ideal components for hard tissue applications. Besides, precise control over interconnecting porosity is of paramount importance for tissue engineering materials. Conventional methods for creating porous scaffolds frequently encounter difficulties in regulating pore size distribution. This study demonstrates the fabrication of gelatin-nano HA scaffolds with uniform porosity using a T-type junction microfluidic device in a single-step process. Significant improvements in control over the pore size distribution are achieved by regulating the flow parameters, resulting in effective and time-efficient manufacturing comparable in quality to the innovative 3D bioprinting techniques. The overall porosity of the scaffolds exceeded 60%, with a remarkably narrow size distribution. The incorporation of nano-HAinto 3D porous gelatin scaffolds successfully induced osteogenic differentiation in stem cells at both the protein and gene levels, as evidenced by the significant increase in osteocalcin (OCN), an important marker of osteogenic differentiation. The OCN levels are 26 and 43 times higher for gelatin and gelatin-HA scaffolds, respectively, compared to the control group.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。