Compressive Strength Testing of Glass-Fibre-Reinforced Tooth Crown Tissues After Endodontic Treatment

根管治疗后玻璃纤维增强牙冠组织的抗压强度测试

阅读:1

Abstract

The objective of this study was to compare the effects of using short and continuous fibres for repairing compression-induced tooth crown damage. Human teeth were used for the study. They were upper medial incisors and maxillary first premolars lost due to periodontal causes. The teeth were divided into two groups with Hahnenkratt and short glass fibres. Teeth compressive strength tests were carried out. Then micro-CT imaging of the teeth and their fractures obtained after compression was performed. The teeth restored with Hahnenkratt's glass fibre posts showed higher compressive strength than the teeth restored using the EverX Posterior material. The tooth's most weakened and sensitive point after endodontic treatment was the cervical area of the tooth. All cracks were parallel to the root canal.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。