Increasing the Corrosion Resistance in the UNS S32750 Super Duplex Steel Welded Joints through Hybrid GTAW-Laser Welding and Nitrogen

通过混合GTAW-激光焊接和氮气处理提高UNS S32750超级双相钢焊接接头的耐腐蚀性

阅读:1

Abstract

The development of techniques to improve the welding of super duplex steels is necessary in order to ensure that the phase balance and properties of the material are not affected during this process. Hybrid arc-laser welding is a perfect combination of the advantages of both processes, producing deeper weld beads with more balanced phases than the pulsed laser process. Here, the objective was to improve the corrosion resistance of UNS S32750 weld beads by increasing the volumetric austenite percentage in the fusion zone (FZ) with a hybrid process of GTAW (gas tungsten arc welding) and pulsed laser Nd-YAG (neodymium-doped yttrium aluminum garnet). Welds were performed in bead on plate conditions with fixed laser parameters and a varying heat input introduced through the GTAW process. Additionally, welds within a nitrogen atmosphere were performed. After base metal characterization, an analysis of the FZ and heat affected zone were performed with optical microscopy, scanning electron microscopy and critical pitting tests (CPT). The synergy between the thermal input provided by the hybrid process and austenite-promoting characteristic of nitrogen led to a balanced volumetric austenite/ferrite fraction. Consequently, the results obtained in CPT tests were better than conventional welding processes, such as laser or GTAW solely.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。