Study on Pyrolysis Characteristics of Phosphate Tailings under H(2)O Atmosphere

H₂O气氛下磷酸盐尾矿热解特性的研究

阅读:1

Abstract

The pyrolysis separation of calcium and magnesium from phosphate tailings is an important process due to its high-value resource utilization. In this paper, aiming to address the problems of high energy consumption, a slow decomposition rate and the low activity of decomposition products in the high-temperature pyrolysis of phosphate tailings, the medium-temperature pyrolysis of phosphate tailings under a H(2)O atmosphere was carried out, and the phase reconstruction and activation of pyrolysis process were discussed. The results showed that compared with N(2), air and CO(2) atmospheres, the pyrolysis process of phosphate tailings in a H(2)O atmosphere was changed from two stages to one stage, the starting decomposition temperature was reduced to 500 °C and the decomposition time was shortened to 30 min. The order of the influence of each factor on the pyrolysis of phosphate tailings was temperature > H(2)O pressure > holding time. Under the optimized pyrolysis conditions, the yield of CaMg(CO(3))(2) decomposition of phosphate tailings into MgO and CaO was 97.3% and 98.1%, respectively, and the reactivity of MgO was 31.6%. The distribution of Ca and Mg elements in the phosphate tailings after pyrolysis showed a negative correlation, and both of them no longer formed associated compounds; Ca mainly existed in the form of Ca(OH)(2), Ca(5)(PO(4))(3)F, CaSiO(3) and CaF(2), and Mg mainly existed in the form of MgO, MgF(2) and Mg(OH)(2).

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。