Effects of Polymer-Curing Agent Ratio on Rheological, Mechanical Properties and Chemical Characterization of Epoxy-Modified Cement Composite Grouting Materials

聚合物-固化剂比例对环氧改性水泥复合灌浆材料流变性能、力学性能和化学特性的影响

阅读:1

Abstract

This study designs and uses water-borne epoxy resin (WBER) and curing agent (CA) to modify traditional cement-based grouting for tunnels. The purpose of this paper is to analyze the rheological and mechanical properties of composite grouting with different ratios of WBER and CA and analyze the modification mechanism by means of chemical characterization to explore the feasibility of WBER as a high-performance modifier for tunnel construction. The composite grouting is prepared by mixing cement paste with polymer emulsion. A series of experiments was carried out to investigate the effects of WBER and CA, including the slump test, viscosity, rheological curve, setting time, bleeding rate, grain size distribution, zeta potential, compressive and splitting tensile strength, X-ray diffraction(XRD), Fourier-transform infrared spectroscopy (FT-IR), and scanning electron microscopy (SEM), on the composite grout. The results show that WBER improves grout fluidity, which decreases in combination with CA, while also reducing the average particle size of the composite grout for a more rational size distribution. Optimal uniaxial (38.9%) and splitting tensile strength (48.7%) of the grout are achieved with a WBER to CA mass ratio of 2:1. WBER accelerates cement hydration, with the modification centered on the reaction between free Ca(2+) and polymer-OH, significantly enhancing the strength, fluidity, and stability of the polymer-modified composite grout compared to traditional cement-based grouting.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。