Effect of Repeated Autoclave on Hardness and Tensile Strength of Polypropylene/Natural Rubber Developed for Rubber Dam Clamp

重复高压釜处理对用于橡胶坝夹的聚丙烯/天然橡胶复合材料的硬度和拉伸强度的影响

阅读:1

Abstract

In this study, we aimed to explore the feasibility of utilizing polypropylene (PP) and natural rubber (NR) blends as alternative materials for rubber dam clamps in dentistry. The hardness of various PP/NR blend ratios was compared to the commercial product SoftClamp(TM). Selected blend ratios exhibiting hardness values resembling rigid plastic were further evaluated for hardness and tensile strength after undergoing 1, 5, and 10 autoclave cycles. One-way ANOVA test results found that the PP/NR blends exhibited significantly lower hardness (p < 0.001) than the commercial SoftClamp(TM). PP/NR ratios of 100/0, 90/10, and 80/20 exhibited hardness levels equivalent to 82%, 80%, and 75% of SoftClamp(TM), respectively. Two-way ANOVA revealed significant reductions in hardness (p < 0.001) and tensile strength (p < 0.001) with increasing NR content across all autoclave cycles. However, post-autoclave assessments at 1, 5, and 10 cycles demonstrated no statistically significant differences in tensile strength (p = 0.058) and hardness (p = 0.52) for PP/NR ratios of 100/0, 90/10, and 80/20 compared to their pre-autoclave states. The NR content within the PP/NR blends decreased hardness and tensile strength, while autoclaving did not significantly affect the hardness and tensile strength of the PP/NR blends.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。