Abstract

By coating surfaces with nano-crystalline diamond (NCD) particles, hydrophilicity can be altered via sidechain modifications without affecting surface texture. The present study aimed to assess the impact of NCD hydrophilicity on machined and rough SLA titanium discs on soft tissue integration, using a rodent model simulating submerged healing. Four different titanium discs (machined titanium = M Titanium, NCD-coated hydrophilic machined titanium = M-O-NCD, sand blasted acid etched (SLA Titanium) titanium, and hydrophilic NCD-coated SLA titanium = SLA O-NCD) were inserted in subdermal pockets of 12 Wistar rats. After one and four weeks of healing, the animals were sacrificed. Biopsies were embedded in methyl methacrylate (MMA), and processed for histology. The number of cells located within a region of interest (ROI) of 10 µm around the discs were counted and compared statistically. Signs of inflammation were evaluated descriptively employing immunohistochemistry. At one week, M-O-NCD coated titanium discs showed significantly higher amounts of cells compared to M Titanium, SLA Titanium, and SLA-O-NCD (p < 0.001). At four weeks, significant higher cell counts were noted at SLA-O-NCD surfaces (p < 0.01). Immunohistochemistry revealed decreased inflammatory responses at hydrophilic surfaces. Within the limits of an animal study, M-O-NCD surfaces seem to stimulate cell proliferation in the initial healing phase, whereas SLA-O-NCD surfaces appeared advantageous afterwards.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。