Investigating the Detachment of Glazed Ceramic Tiles Used in Buildings: A Brazilian Case Study.

调查建筑物中使用的釉面陶瓷砖的脱落情况:以巴西为例

阅读:10
作者:Sahade Renato Freua, Leal Priscila R M, Lima Sérgio S, da Silva Paulo Sérgio, Lima Carlos R C
Ceramic detachments in cladding systems are indicative of adhesion loss between the ceramic tiles and the substrate or its adhesive mortar due to inadequate quality workmanship, the quality of the adhesive mortar or that of the ceramic material, whether acting simultaneously or not. The shear stresses resulting from the ceramic tiles' expansion due to humidity accelerate this process. There is a shortage of studies on the quality of ceramic tiles and adhesive mortars. This study conducted elemental, physical and microstructural characterization tests on ceramic tiles and adhesive mortars that showed detachment up to two years after being laid. At first glance, the adhesive mortar samples had adequate traits and degree of hydration. The ceramic tiles, on the other hand, showed high porosity and high levels of amorphous and poorly sintered materials, with no crystalline phase. In a second analysis, scanning electron microscopy (SEM) tests associated with boiling plus autoclave moisture expansion tests executed on unused ceramic pieces of the same conformation proved to be more suitable for predicting expansion potential than standard tests. Due to the costs and difficulties in accessing and analyzing the SEM tests, chemical analysis of the ceramic tiles was executed using X-ray fluorescence (XRF) to assess the presence of the amorphous silica (free quartz) and alkaline oxides. Together with pressure and temperature determination tests (autoclave), they may represent another alternative that is easier to access and more cost-effective for predicting future expansion.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。