Effect of Ethylene diamine tetra acetic acid and sodium hypochlorite solution conditioning on microtensile bond strength of one-step self-etch adhesives.

阅读:8
作者:Kasraei Shahin, Azarsina Mohadese, Khamverdi Zahra
BACKGROUND: Attempts to improve bond strength of self-etch adhesives can enhance the durability of composite restorations. AIMS: The aim of the present study was to evaluate the effect of collagen and smear layer removal with sodium hypochlorite solution (NaOCl) and EDTA on micro-tensile bond strength (μTBS) of self-etch adhesives to dentin. SETTINGS AND DESIGN: It was an in-vitro study. MATERIALS AND METHODS: Seventy-two teeth were divided into eight groups and their crowns were ground perpendicular to their long axis to expose dentin. The teeth were polished with silicon-carbide papers. The groups were treated as follows: No conditioning, 0.5-M EDTA conditioning, 2.5% NaOCl conditioning, NaOCl + EDTA conditioning. The surfaces were rinsed and blot-dried. Clearfil S3 and I-Bond were applied according to manufacturers' instructions and restored with Z100 composite. After 500 cycles of thermo-cycling between 5°C and 55°C, the samples were sectioned and tested for μTBS. STATISTICAL ANALYSIS: Data were analyzed by two-way ANOVA and Tukey-HSD test. RESULTS: The highest μTBS was recorded with Clearfil S3 + NaOCl + EDTA, and the lowest was recorded with I-Bond without conditioning. μTBS in EDTA-and EDTA + NaOCl-treated groups was significantly higher than the control and NaOCl-conditioned groups. CONCLUSIONS: Application of EDTA or EDTA + NaOCl before one-step self-etch adhesives increased μTBS.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。