Mesoporous Silica with an Alveolar Construction Obtained by Eco-Friendly Treatment of Rice Husks

通过对稻壳进行环保处理制备具有蜂窝状结构的介孔二氧化硅

阅读:2

Abstract

The high silicon content in rice plant waste, specifically rice husks, makes this waste by-product attractive for the extraction and valorization of silicon oxide, which is widely used as an inert support in catalysis, drug delivery and molecular sieving. The procedures currently used for the treatment of plant biomass make extensive use of mineral acids (HCl, H(2)SO(4), HNO(3)), which, besides them being potential environmental pollutants, reduce the yield and worsen the chemical-physical properties of the product. In this study, an evaluation of the easy treatment of rice husks by benchmarking different, more eco-friendly carboxylic acids in order to obtain a mesoporous SiO(2) with an alveolar structure and a relatively high surface area and pore volume (300-420 m(2)/g, 0.37-0.46 cm(3)/g) is presented. The obtained mesoporous silicas are characterized by worm-like pores with a narrow size distribution and a maximum in the range of 3.4-3.5 nm. The mesoporous structure of the obtained materials was also confirmed by TEM. The complete removal of the organic part of the rice husks in the final materials was evidenced by thermogravimetric analysis. The high purity of the obtained mesoporous silica was detected using ICP analysis (98.8 wt. %). The structure peculiarities of the obtained mesoporous silicas were also characterized by solid-state NMR and ATR-FTIR spectroscopies. The morphology of the mesoporous silica was investigated by SEM.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。