Single Particle Assays to Determine Heterogeneities within Fluid Catalytic Cracking Catalysts

单颗粒分析确定流化催化裂化催化剂内的异质性

阅读:7
作者:Anne-Eva Nieuwelink, Marjolein E Z Velthoen, Yoni C M Nederstigt, Kristel L Jagtenberg, Florian Meirer, Bert M Weckhuysen

Abstract

Fluid catalytic cracking (FCC) is an important process in oil refinery industry to produce gasoline and propylene. Due to harsh reaction conditions, FCC catalysts are subject to deactivation through for example, metal accumulation and zeolite framework collapse. Here, we perform a screening of the influence of metal poisons on the acidity and accessibility of an industrial FCC catalyst material using laboratory-based single particle characterization that is, μ-XRF and fluorescence microscopy in combination with probe molecules. These methods have been performed on density-separated FCC catalyst fractions, allowing to determine interparticle heterogeneities in the catalyst under study. It was found that with increasing catalyst density and metal content, the acidity and accessibility of the catalyst particles decreased, while their distribution narrowed with catalyst age. For example, particles containing high Ni level possessed very low acidity and were hardly accessible by a Nile Blue dye. Single catalyst particle mapping identifies minority species like the presence of a phosphated zeolite ZSM-5-containing FCC additive for selective propylene formation, catalyst particles without any zeolite phase and catalyst particles, which act as a trap for SOx .

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。