Conclusion

Fluoride ions were released cumulatively over the entire test period for all products. When comparing the two products from the same company (Fuji ORTHO LC vs. Fuji ORTHO from GC Orthodontics Europe GmbH and Meron Plus QM vs. Meron from VOCO GmbH, Mannheim, Germany), it can be said that the resin-modified GICs have a higher release than conventional GICs. The highest individual fluoride release of all GICs was at 24 hours. A general statement, whether resin-modified or conventional GICs have a higher release of fluoride cannot be made.

Methods

The resin-modified GICs Fuji ORTHO LC (GC Orthodontics), Meron Plus QM (VOCO), as well as the conventional GICs Fuji ORTHO (GC Orthodontics), Meron (VOCO) and Ketac Cem Easymix (3M ESPE) were tested in this study. The different types of GICs were applied to hydroxyapatite discs according to the manufacturer's instructions and stored in a solution of TISAB III (Total Ionic Strength Adjustment Buffer III) and fluoride-free water at 37°C. Fluoride measurements were made after 5 minutes, 2 hours, 24 hours, 14 days, 28 days, 2 months, 3 months and 6 months. One factor analysis of variance (ANOVA) was used for the overall comparison of the cumulative fluoride release (from measurement times of 5 minutes to 6 months) between the different materials with the overall level of significance set to 0.05. Tukey's post hoc test was used for post hoc pairwise comparisons in the cumulative fluoride release between the different materials.

Results

The cumulative fluoride release (mean ± sd) in descending order was: Fuji ORTHO LC (221.7 ± 10.29 ppm), Fuji ORTHO (191.5 ± 15.03 ppm), Meron Plus QM (173.0 ± 5.89 ppm), Meron (161.3 ± 7.84 ppm) and Ketac Cem Easymix (154.6 ± 6.09 ppm) within 6 months. Analysis of variance detected a significant difference in the cumulative fluoride release between at least two of the materials (rounded p-value < 0.001). Pairwise analysis with Tukey's post hoc test showed a significant difference in the cumulative fluoride release for all the comparisons except M and MPQM (p = 0.061) and KCE and M (p = 0.517).