Introducing biomimetic shear and ion gradients to microfluidic spinning improves silk fiber strength

将仿生剪切和离子梯度引入微流体纺丝可提高丝纤维强度

阅读:12
作者:David Li, Matthew M Jacobsen, Nae Gyune Rim, Daniel Backman, David L Kaplan, Joyce Y Wong

Abstract

Silkworm silk is an attractive biopolymer for biomedical applications due to its high mechanical strength and biocompatibility; as a result, there is increasing interest in scalable devices to spin silk and recombinant silk so as to improve and customize their properties for diverse biomedical purposes (Vepari and Kaplan 2007 Prog. Polym. Sci. 32 ). While artificial spinning of regenerated silk fibroins adds tunability to properties such as degradation rate and surface functionalization, the resulting fibers do not yet approach the mechanical strength of native silkworm silk. These drawbacks reduce the applicability and attractiveness of artificial silk (Kinahan et al 2011 Biomacromolecules 12 ). Here, we used computational fluid dynamic simulations to incorporate shear in tandem with biomimetic ion gradients by coupling a modular novel glass microfluidic device to our previous co-axial flow device. Fibers spun with this combined apparatus demonstrated a significant increase in mechanical strength compared to fibers spun with the basic apparatus alone, with a three-fold increase in Young's modulus and extensibility and a twelve-fold increase in toughness. These results thus demonstrate the critical importance of ionic milieu and shear stress in spinning strong fibers from solubilized silk fibroin.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。