Resolution of Lithium Deposition versus Intercalation of Graphite Anodes in Lithium Ion Batteries: An In Situ Electron Paramagnetic Resonance Study

锂离子电池中石墨负极锂沉积与插层的分辨:原位电子顺磁共振研究

阅读:1

Abstract

In situ electrochemical electron paramagnetic resonance (EPR) spectroscopy is used to understand the mixed lithiation/deposition behavior on graphite anodes during the charging process. The conductivity, degree of lithiation, and the deposition process of the graphite are reflected by the EPR spectroscopic quality factor, the spin density, and the EPR spectral change, respectively. Classical over-charging (normally associated with potentials ≤0 V vs. Li(+) /Li) are not required for Li metal deposition onto the graphite anode: Li deposition initiates at ca. +0.04 V (vs. Li(+) /Li) when the scan rate is lowered to 0.04 mV s(-1) . The inhibition of Li deposition by vinylene carbonate (VC) additive is highlighted by the EPR results during cycling, attributed to a more mechanically flexible and polymeric SEI layer with higher ionic conductivity. A safe cut-off potential limit of +0.05 V for the anode is suggested for high rate cycling, confirmed by the EPR response over prolonged cycling.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。