Surface Roughness of Glass Ionomer Cements after Application of Different Polishing Techniques

采用不同抛光技术后玻璃离子水门汀的表面粗糙度

阅读:6
作者:Ante Miličević, Kristina Goršeta, Raimond Nv van Duinen, Domagoj Glavina

Conclusion

Based on the obtained results, it can be concluded that the smoothest surface roughness is achieved by the Mylar strip. Some types of Glass Ionomer Cements can obtain better surface polishing with heat treatment (thermo-curing).

Methods

Two polishing systems (Tungsten carbide burs and Sof-Lex discs) were used on two types of GIC (Equia Fil and Ketac Molar Universal). Bluephase 16i LED (Vivadent, Schaan Liechtenstein) light was used for the specimens treated with heat (thermo-curing). Samples without heat treatment are left for 10 minutes to chemically cure. Surface profilometar was used for measuring the mean surface roughness value (Ra).

Results

Group with Mylar strip (control group) of each material showed the lowest (Ra) value. The Equia Fil material samples treated with heat (thermo-curing) achieved lower surface roughness values (Ra), and showed lower surface roughness values (Ra) after polishing with a Sof-Lex discs (p<0.05). The results for Ketac Molar Universal samples showed no statistically significant difference (p>0.05) between polishing with Sof-Lex discs and Tungsten carbide burs.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。