Rationally Designed Eugenol-Based Chain Extender for Self-Healing Polyurethane Elastomers

合理设计的丁香酚基扩链剂用于自修复聚氨酯弹性体

阅读:1

Abstract

Bio-based polyurethane (PU) has recently drawn our attention due to the increasing interest in sustainability and the risks involved with petroleum depletion. Herein, bio-based self-healing PU with a novel polyol, i.e., eugenol glycol dimer (EGD), was synthesized and characterized for the first time. EGD was designed to have pairs of primary, secondary, and aromatic alcohols, which all are able to be involved in urethane bond formation and to show self-healing and antioxidant effects. EGD was incorporated into a mixture of the prepolymer of polyol (tetramethylene ether glycol) and 4,4'-methylene diphenyl diisocyanate to synthesize PU. EGD-PU showed excellent self-healing properties (99.84%), and it maintained its high self-healing property (84.71%) even after three repeated tests. This dramatic self-healing was induced through transcarbamoylation by the pendant hydroxyl groups of EGD-PU. The excellent antioxidant effect of EGD-PU was confirmed by 2,2-diphenyl-1-picrylhydrazyl analysis. Eugenol-based EGD is a promising polyol chain extender that is required in the production of bio-based, self-healing, and recyclable polyurethane; therefore, EGD-PU can be applied to bio-based self-healable films or coating materials as a substitute for petroleum-based PU.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。