In Vitro Evaluation of a Semi-Autologous Fibrin Sealant for Surgical Applications

体外评价半自体纤维蛋白密封剂在外科手术中的应用

阅读:1

Abstract

Surgical success relies on precise tissue approximation using sutures, clips, or staples. Fibrin sealant provides a user-friendly alternative, saving time and maintaining tissue integrity. Yet, its cost and potential bioburden risk are notable drawbacks. To address these concerns, a semi-autologous fibrin sealant is produced from human cryoprecipitate and compared it to a commercial fibrin sealant. The microstructure of the semi-autologous sealant closely resembles the commercial one. Initially, the commercial sealant has superior bonding strength, however, over time, both demonstrate strong adhesive properties. Moreover, when the two sealants contain equivalent fibrinogen concentrations, they show similar bonding strength and rheological properties, including thixotropic behavior, which is essential for their application as bioadhesives. Notably, it is discovered that the mechanical properties of the adhesive are mainly governed by the fibrinogen concentration, with minimal impact of other blood components. This understanding paves the way for the development of an efficient method to boost fibrinogen in blood without extensive separation. This study indicates semi-autologous fibrin glue matches commercial sealant in adhesive properties. This may offer several advantages, such as reduced bioburden, costs, improved immunomodulation, and reduced hypersensitivity and virus transmission risks. These findings hold promising prospects for enhancing the wound healing process in various medical conditions.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。