Effect of Pulpal Base, Restorative Material, and Preparation Type on Marginal and Internal Fit and Fracture Strength of Endocrowns

牙髓基质、修复材料和预备类型对牙冠边缘和内部密合度及抗折强度的影响

阅读:2

Abstract

The aim of this innovative study was to investigate the feasibility of a modified butt joint preparation with two grooves instead of a ferrule when root dentin tissue is limited in mandibular molars. It was also investigated to what extent the effect of these treatment options on marginal and internal fit and fracture strength (FS) varied according to the type of material and whether or not a fiber ribbon was used at the base. Marginal and internal fit were evaluated using the triple-scan protocol. Statistical analysis was conducted via a three-way analysis of variance (ANOVA). The absolute marginal discrepancy (AMD), marginal discrepancy, and overall fit values for the ceramic group were 127 μm, 108 μm, and 120 μm, respectively, while corresponding values for the hybrid ceramic group were 139 μm, 116 μm, and 130 μm (p < 0.05). The mean FS recorded for ceramic restorations was 662 N, whereas hybrid ceramic restorations demonstrated a significantly higher FS of 903 N (p < 0.001). When material type was assessed independently of preparation design and base configuration, both ceramic and hybrid ceramic exceeded the predefined clinical acceptability threshold for AMD; however, they remained within acceptable limits for the remaining parameters. Among the evaluated configurations, hybrid ceramic restorations incorporating ferrules and fiber-reinforced bases exhibited the highest FS values, whereas ceramic restorations with modified biological widths and lacking fiber reinforcement yielded the lowest FS values.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。