Conclusions
Aggregation of cells after storage at 25 °C in LR-3T-5D may be suppressed by increasing the storage volume and cell density as well as by incorporating nitrogen replacement, which lowers the pO2 in the solution.
Methods
We first examined the effects of storage temperature and time on the aggregation and viability of hADSCs stored in LR and LR-3T-5D. The cells were stored at 5 °C or 25 °C for various times up to 24 h. We then evaluated the effects of storage volume (250-2,000 μL), cell density (2.5-20 × 105 cells/mL), and nitrogen gas replacement on aggregation, oxygen partial pressure (pO2), and viability of hADSCs stored for 24 h at 25 °C in LR-3T-5D.
Results
When stored in LR-3T-5D, viability did not change under either condition compared with pre-storage, but the cell aggregation rate increased significantly with storage at 25 °C for 24 h (p<0.001). In LR, the aggregation rate did not change under either condition, but cell viability decreased significantly after 24 h at both 5 °C and 25 °C (p < 0.05). The cell aggregation rates and pO2 tended to decrease with increasing solution volume and cell density. Nitrogen gas replacement significantly decreased the cell aggregation rate and pO2 (p < 0.05). However, there were no differences in viability among cells stored under conditions of different storage volumes, densities, and nitrogen gas replacement. Conclusions: Aggregation of cells after storage at 25 °C in LR-3T-5D may be suppressed by increasing the storage volume and cell density as well as by incorporating nitrogen replacement, which lowers the pO2 in the solution.