Biodegradable poly(caprolactone fumarate) 3D printed scaffolds for segmental bone defects within the Masquelet technique.

采用 Masquelet 技术治疗节段性骨缺损的可生物降解聚(己内酯富马酸酯)3D 打印支架

阅读:5
作者:Astudillo Potes Maria D, Mitra Indranath, Hanson Kari, Camilleri Emily T, Gaihre Bipin, Shafi Mahnoor, Hamouda Abdelrahman, Lu Lichun, Elder Benjamin D
Segmental bone defects, often clinically treated with nondegradable poly(methylmethacrylate) (PMMA) in multistage surgeries, present a significant clinical challenge. Our study investigated the efficacy of 3D printed biodegradable polycaprolactone fumarate (PCLF)/PCL spacers in a one-stage surgical intervention for these defects, focusing on early bone regeneration influenced by spacer porosities. We compared nonporous PCLF/PCL and PMMA spacers, conventionally molded into cylinders, with porous PCLF/PCL spacers, 3D printed to structurally mimic segmental defects in rat femurs for a 4-week implantation study. Histological analysis, including tissue staining and immunohistochemistry with bone-specific antibodies, was conducted for histomorphometry evaluation. The PCLF/PCL spacers demonstrated compressive properties within 6 ± 0.5 MPa (strength) and 140 ± 15 MPa (modulus). Both porous PCLF/PCL and Nonporous PMMA formed collagen-rich membranes (PCLF/PCL: 92% ± 1.3%, PMMA: 86% ± 1.5%) similar to those induced in the Masquelet technique, indicating PCLF/PCL's potential for one-stage healing. Immunohistochemistry confirmed biomarkers for tissue regeneration, underscoring PCLF/PCL's regenerative capabilities. This research highlights PCLF/PCL scaffolds' ability to induce membrane formation in critical-sized segmental bone defects, supporting their use in one-stage surgery. Both solid and porous PCLF/PCL spacers showed adequate compressive properties, with the porous variants exhibiting BMP-2 expression and woven bone formation, akin to clinical standard PMMA. Notably, the early ossification of the membrane into the pores of porous scaffolds suggests potential for bone interlocking and regeneration, potentially eliminating the need for a second surgery required for PMMA spacers. The biocompatibility and biodegradability of PCLF/PCL make them promising alternatives for treating critical bone defects, especially in vulnerable patient groups.

特别声明

1、本页面内容包含部分的内容是基于公开信息的合理引用;引用内容仅为补充信息,不代表本站立场。

2、若认为本页面引用内容涉及侵权,请及时与本站联系,我们将第一时间处理。

3、其他媒体/个人如需使用本页面原创内容,需注明“来源:[生知库]”并获得授权;使用引用内容的,需自行联系原作者获得许可。

4、投稿及合作请联系:info@biocloudy.com。